Corrosion of AISI 316 and AISI 304 stainless steel with iodine vapor [electronic resource]
The weight loss of stainless steel in corrosion with iodine vapor was studied at 500 to 1000 deg C and an iodine vapor pressure range of 0.05 to 0.5 mm Hg, using a thermobalance. In the initial stage of corrosion, the weight loss rate is largely influenced by solution treatment or surface treatment;...