Relationship between swelling and irradiation creep in cold-worked PCA stainless steel irradiated to ∼178 dpa at ∼400°C [electronic resource]
The eighth and final irradiation segment for pressurized tubes constructed from the fusion Prime Candidate Alloy (PCA) has been completed in FFTF. At 178 dpa and ∼400°C, the irradiation creep of 20% cold-worked PCA has become dominated by the {open_quotes}creep disappearance{close_quotes} phenomenon...