PREPARATION OF ThO$sub 2$ FOR HOMOGENEOUS REACTOR BLANKET USE [electronic resource]

The flowsheet for making thorium oxide in 284-lb batches provides for adding 1M oxalic acid to 1M and step-calcined to 1600 deg C for 4 hr. After classification the final product has an average particle size close to 1 mu with less than 2 wt % larger than 5 mu . In laboratory studies thorium oxalate...

Full description

Saved in:
Bibliographic Details
Online Access: Online Access (via OSTI)
Corporate Author: Oak Ridge National Laboratory (Researcher)
Format: Government Document Electronic eBook
Language:English
Published: Oak Ridge, Tenn. : Oak Ridge, Tenn. : Oak Ridge National Laboratory. ; distributed by the Office of Scientific and Technical Information, U.S. Department of Energy, 1958.
Subjects:

Internet

Online Access (via OSTI)

Online

Holdings details from Online
Call Number: E 1.99:ornl-2509
E 1.99:ornl-2509 Available